Inks and Adhesives for Compostable Packaging: 3 Realistic Boundaries—Why Paper Is Not a Problem, but Ink and Glue Get Stuck at EN 13432 Certification
💡 💡 At a Glance
When compostable packaging certification is rejected, the problem often lies not in the paper, but in the ink and adhesive. There are three real boundaries: First, the ink layer is subject to heavy-metal limits and pigment migration restrictions—plant-based binders do not mean plant-based pigments, and inorganic pigments containing cadmium, lead, or chromium can be used in vegetable-based inks; certification evaluates the paper-and-ink combination. Second, the adhesive layer must meet the requirements for biodegradability, not merely compostability; heat-seal adhesives are often multilayer coextrusions, and the OECD 301 biodegradation data for the intermediate bonding layer are held by the adhesive manufacturer, so an “eco-friendly heat-seal adhesive” does not necessarily pass testing. Third, the item submitted for testing is the complete packaging system. Paper, ink, coatings, adhesive, labels, and caps all count; if any item is omitted, the conclusion does not cover the final product. For example, a PET label can turn the entire package from compostable into mixed material. Before accepting this order, the printer should obtain three documents: proof of the substrate’s certification status, the ink composition and heavy-metal and biodegradation reports for the specific model and batch, and the BOM and biodegradation evidence covering all attachments. Certification takes four to six weeks and must be scheduled before mass production begins.
Paper is environmentally friendly, but the cups are not certified.
In April 2026, a plant-based milk customer contacted us about printing 200,000 compostable paper cups holding 250 ml each.
They had chosen the materials themselves: sugarcane-bagasse paper cups, printing with soy-based ink, and hot-seal film for bonding. The entire chain appeared clean—the paper came from agricultural waste, the ink was plant-based, and the film was marketed as compostable.
The sample itself was fine. However, when it was sent for certification, the laboratory rejected it, citing a very direct reason:“No evidence was provided that the bonding layer of the sample meets the biodegradation requirements; additional testing is needed for the heavy-metal limits of the pigments in the printed layer.”
The client was deeply frustrated:“All of our materials are environmentally friendly.”
The issue is that “environmentally friendly” and “passing EN 13432 certification” are two different things. The former is an adjective, while the latter is a quantifiable standard. Sugarcane-bagasse paper can pass because its degradation pathway is clear; whether the ink and adhesive pass depends on the specific pigment system and degradation data—Not all printing inks qualify, and not all heat-seal films qualify either..
Boundary 1: At the ink layer, EN 13432 regulates heavy metals and the migration of colorants.
Compostable packaging entering soil or an industrial composting facility is broken down, fermented, and turned into compost. Therefore, if the ink contains heavy metals, they will return to the soil with the compost; if colorants migrate under composting conditions, they will affect the compliance of the final compost product.
EN 13432’s core requirements for the printing layer focus on two areas:
First,Heavy metal limits.Lead, cadmium, mercury, hexavalent chromium, and other substances are subject to total quantity limits across all packaging components, and ink is one of the explicitly listed components. Phthalocyanine-based blue and green inks and inks containing chrome yellow are commonly used.
Second, regardingColorant migrationUnder simulated composting conditions, the printed layer must not exhibit noticeable color bleeding.
Vegetable-based ink does not automatically mean it will pass inspection. Soybean-based ink addressesVOC and vegetable oil ratioSuch issues. Its relationship to heavy-metal limits is that a vegetable-based binder does not mean a vegetable-based pigment. Inorganic pigments containing heavy metals, such as cadmium yellow and lead red, can be used in vegetable-based inks.
Therefore, what customers should ask suppliers is not “Is your ink vegetable-based?” but three questions:What is the pigment system in this ink? Is there a heavy-metal test report? Does the report cover this specific ink?
Printing plants bear an additional responsibility regarding print suitability: compostability certification often requiresthe finished product or semi-finished product to be tested as a whole,which means that, after the ink is printed onto the paper, the paper-and-ink combination becomes the object being evaluated. An excessively thick ink layer or overly heavy overprinting may alter the evaluation results.
The second boundary: At the adhesive layer, what is required is "biodegradability," not "compostability."
This is the second boundary that is particularly easy to overlook.
In EN 13432, theorganic componentsof packaging have an overall requirement: they must be biodegradable. The assessment process generally begins with the OECD 301 aerobic biodegradability test (typically requiring at least 60% biodegradation within 28 days), followed by the ISO 14855 soil burial test for certain materials, and by complete biodegradation verification related to ISO 16929 under composting conditions.
There is a specific number that is often misread:90%Many customers treat “degradable within 90 days” as a certification threshold. In reality, 90 days is a cycle condition in certain testing methods, not a pass/fail line. The threshold is whether the biodegradation rate reaches the specified percentage within the prescribed period.
The problem with adhesives is that customers often do not control their composition. A paper cup supplier may give you an “eco-friendly heat-seal adhesive,” but heat-seal adhesives are often multilayer co-extrusions—the outer layer may be compostable polyester or paper-based, while the middle layer is an adhesive layer. Whether that adhesive layer is biodegradable and compliant with OECD 301 depends entirely on the adhesive manufacturer.
What ultimately happened to those 200,000 paper cups: the customer obtained the adhesive supplier’s complete BOM and third-party test reports and confirmed that the adhesive layer met the requirements; for the ink, they changed the pigment system, added a heavy-metal test report, and passed the retest.
It took five weeks in total.“The customer chooses the materials, so the customer also has to request the reports.”This was the most practical lesson I learned from that order handled by the sales representative.
Boundary 3: The object submitted for testing is not the same as the object the customer thinks is being submitted.
This is the third boundary, and it is the one most likely to make the entire project a wasted trip.
Submitting for testing does not mean submitting “a piece of paper and a cup.” EN 13432 evaluatesa complete packaging system,including the substrate, printing layer, coating, adhesive, label, lid, and closure. Therefore, all of the following can affect the certification result:
- The label on the cupThe label— if it is a sticker, does the sticker’s adhesive count as a separate component?
- Cup lid—If the lid is plastic, the compostability of the entire package is directly affected.
- Ink—The evaluation results for the same paper cup may differ when printed in dark and light colors.
- Screen printing / Inkjet printing—Different printing methods have different ink layer thicknesses and compositions.
There was another issue with our order: the customer originally planned to add a PET label to the paper cup to highlight the logo. After the test results came back, the PET label changed the entire package from “compostable” to “mixed-material non-compostable.” In the end, they switched to direct screen printing on the cup.
Therefore, before submitting the samples for testing, the following must be done:Submit a complete bill of materials for the final finished product, with nothing omitted.If even one item is missing from the list, the test results will not represent the final product.
Before accepting this order, which three materials should the printing plant request from the customer?
Without these three documents, the printing plant’s production schedule is nothing more than a castle in the air:
First, proof of the certification status of the substrate material.Is it paper that has already obtained EN 13432 certification, or material that meets the requirements but is still awaiting certification? The two options require 4 to 8 more weeks.
Second, a complete composition statement for this batch of ink, along with a heavy metals test report and a biodegradability test report.The reports must correspond to the specific model and specific batch range, rather than merely stating that all of our inks have reports.
The BOM for the adhesive (and all attachments such as lids and labels), together with corresponding evidence of degradability.It must be possible to trace every layer. One specific question: Is the heat-seal adhesive coextruded or a single layer?
Also, a reminder about the production schedule:Certification testing usually requires samples made using the mass-production process., rather than prototypes. Therefore, the process is “materials complete → produce mass-production samples → submit for testing → pass → start production.” The four to six weeks required for testing must be scheduled before printing production, not after it.
Many customers ask:“Can we print part of it first and print the rest after certification is completed?”This is not recommended. Certification is evaluated based on the final formulation and process. If the materials used in the first printed batch are not completely consistent with the submitted samples, the certification will not cover that batch. You will then have to either scrap the entire batch or submit it for testing again.
Further reading
The certification thresholds for compostable packaging themselves and the differences between the two sets of standards:Compostable packaging certification (EN 13432 / ASTM D6400): a mandatory threshold for products to be sold in Europe and the United States
The most commonly confused elements among the three labels:Further confusion between the three types of labels—biodegradable, compostable, and recyclable
The food-contact compliance of the ink itself is a separate issue:The real boundaries of the three categories of inks for food contact under GB 4806.14-2023
Adhesive selection and design for disassembly:Three realistic boundaries of packaging “adhesives”: structural bonding / disassemblable bonding / label transfer
Another approach to making the entire package recyclable:Three realistic boundaries of “recyclable packaging design” (Recycle-Ready)
FAQ
You're using plant-based ink and compostable paper. Why is the certification still being denied?
Because “eco-friendly” is not a certification standard. EN 13432 focuses on measurable criteria: heavy-metal limits for ink components, colorant migration under simulated composting conditions, and the biodegradation rate of organic components such as adhesives. A plant-based vehicle does not mean plant-based pigments; inorganic pigments containing cadmium, lead, or chromium can be used in plant-based inks. If a heat-seal adhesive is a multilayer coextrusion, whether the intermediate bonding layer is biodegradable depends on the adhesive manufacturer, not the paper-cup supplier.
Does EN 13432 require complete biodegradation within 90 days?
Ninety days is a cycle condition in certain testing methods, not a pass threshold. Organic components are usually first subjected to the OECD 301 aerobic biodegradation test, which requires the specified proportion to be reached within 28 days (the commonly cited threshold is 60% or more); composting conditions also require supplemental full biodegradation verification under ISO 16929. Treating “degradable within 90 days” as a certification threshold is a widespread misconception.
For inspection, do we only need to send the paper and ink? Do the glue, lids, and labels need to be sent as well?
They need to be delivered together. EN 13432 evaluates a complete packaging system, including the substrate, printing layer, coating, adhesive, label, lid, and closure. If any item is missing from the submitted test materials, the test results will not represent the final product. Simply adding a PET label with a logo to a paper cup turns the entire packaging from compostable to non-compostable mixed material.
Can we print part of it first and print the rest after certification is completed?
Not recommended. Certification is assessed based on the final formula and process. If the first printed batch and the submitted sample do not match exactly in materials, the certification does not cover that batch, and the result will be either scrapping the entire batch or resubmitting it for testing. The correct sequence is: finalize materials → produce samples using the mass-production process → submit for testing → pass → start mass production.
What responsibility does the printing company bear regarding certification?
The printing factory is responsible for faithfully printing the approved materials: ink models must not be substituted without authorization, ink layer thickness and overprinting must remain within the range of the submitted samples, the accessory list must follow the submitted version, and evidence of the production run must be retained to prove that the production matches the submitted samples. At the same time, the printing factory must ensure printability, as excessively thick ink layers or overly deep overprinting may alter the overall evaluation results.
Will the certification results differ between light-colored and dark-colored printing on the same batch of paper cups?
It is possible. The amounts of components in the printing layer and the number of overprints vary with color depth. Darker colors require more ink, and the amounts of pigments and heavy metals introduced also vary accordingly. The submitted samples must be consistent with the printing method, number of colors, and color depth of the final mass-production version. Submitting samples in a light color while mass-producing in a dark color will raise questions during the review.
📚 📚 Related Recommendations
Need a Custom Packaging Solution?
Learn more about packaging, or consult directly for a custom solution and quote